保定環氧地坪為什么會出現漆膜腫脹、表面看起來漆膜不完整。表面的光亮度也不是很好。并且分布的不是很均勻。保定環氧地坪出現漆膜腫脹的原因在于,底面的涂料跟基本面容相差很差,脫離漆未干,或者是里面還有液體的存在。分布的是不是均勻等。如果說保定環氧地坪進行施工的時候,漆膜根本沒有干透,或者是上面涂上的底層,還是潮濕的狀態中。這樣在進行選擇材料的時候就需要選擇跟面涂相結合的材料,不然當漆膜受到鹽堿性作用的時候還是會引起漆膜腫脹。
Why does the epoxy floor appear swelling of paint film and incomplete film on the surface? The surface brightness is not very good. And the distribution is not very uniform. The reason for the swelling of the paint film on the epoxy floor is that the paint on the bottom surface is very different from the basic surface, leaving the paint dry, or there is a liquid in it. The distribution is not uniform. If the epoxy floor construction, the film did not dry through, or the top coated on the bottom, or in the wet state. In this way, when choosing the material, we need to choose the material which combines with the surface coating. Otherwise, when the film is affected by salinity and alkalinity, it will still cause the film swelling.